MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Asahi Kasei Leona™ FR250 Polyamide 66, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: Applications: Automotive parts, electrical & electronic parts, parts for office furnishings.

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccDry as Molded; ASTM D792
Density 1.15 g/cc0.0415 lb/in³Dry as Molded; ISO 1183
Moisture Absorption at Equilibrium 2.8 %
@Temperature 23.0 °C
2.8 %
@Temperature 73.4 °F
50% RH
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9393Dry as Molded; ISO 2039
Tensile Strength at Break 46.0 MPa6670 psiDry as Molded; ISO 527
 78.0 MPa11300 psiConditioned at 50% RH; ISO 527
Tensile Strength 48.0 MPa6960 psiConditioned at 50% RH; ASTM D638
 82.0 MPa11900 psiDry as Molded; ASTM D638
Elongation at Break 11 %11 %Dry as Molded; ISO 527
 43 %43 %Conditioned at 50% RH; ISO 527
Tensile Modulus 0.800 GPa116 ksiConditioned at 50% RH; ISO 527
 2.90 GPa421 ksiDry as Molded; ISO 527
Flexural Strength 41.0 MPa5950 psiConditioned at 50% RH; ISO 178
 105 MPa15200 psiDry as Molded; ISO 178
Flexural Modulus 1.00 GPa145 ksiConditioned at 50% RH; ISO 178
 2.80 GPa406 ksiDry as Molded; ISO 178
Izod Impact, Notched 0.450 J/cm0.843 ft-lb/inDry as Molded; ASTM D256
 1.80 J/cm3.37 ft-lb/inConditioned at 50% RH; ASTM D256
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²Dry as Molded; ISO 179
 1.70 J/cm²8.09 ft-lb/in²Conditioned at 50% RH; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FDry as Molded; ISO 75
Oxygen Index 28 %28 %Dry as Molded; ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASAHI8161 / 221188

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.