MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Akro-Plastic Akromid® A3 1 FR black (3051) Nylon 66, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: Flame Retardant Compound. UL 94 V0 at 0.8 mm with good strength and flow. PA 6.6 FR (30).

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.013 - 0.016 cm/cm0.013 - 0.016 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.013 - 0.016 cm/cm0.013 - 0.016 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.0 MPa7980 psi5 mm/min. Conditioned; ISO 527-2
 83.0 MPa12000 psi5 mm/min. Dry as Molded; ISO 527-2
Elongation at Break >= 5.0 %>= 5.0 %5 mm/min. Dry as Molded; ISO 527-2
 >= 20 %>= 20 %5 mm/min. Conditioned; ISO 527-2
Tensile Modulus 1.50 GPa218 ksi1 mm/min. Conditioned; ISO 527-2
 3.50 GPa508 ksi1 mm/min. Dry as Molded.; ISO 527-2
Charpy Impact Unnotched  7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
Dry as Molded; ISO 179-1/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179-1/1eA
Charpy Impact, Notched  0.450 J/cm²
@Temperature 23.0 °C
2.14 ft-lb/in²
@Temperature 73.4 °F
Dry as Molded; ISO 179-1/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index >= 600 V>= 600 VConditioned. Test solution A; IEC 60112
 >= 600 V>= 600 VDry as Molded. Test solution A; IEC 60112
Hot Wire Ignition, HWI  7.0 - 15 sec
@Thickness 0.800 mm
7.0 - 15 sec
@Thickness 0.0315 in
Conditioned; UL 746A
 7.0 - 15 sec
@Thickness 0.800 mm
7.0 - 15 sec
@Thickness 0.0315 in
Dry as Molded; UL 746A
High Amp Arc Ignition, HAI  >= 120 arcs
@Thickness 0.800 mm
>= 120 arcs
@Thickness 0.0315 in
Conditioned; UL 746A
 >= 120 arcs
@Thickness 0.800 mm
>= 120 arcs
@Thickness 0.0315 in
Dry as Molded; UL 746A
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FDry as Molded. DES, 10°C/min; DIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FDry as Molded; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FDry as Molded; ISO 75
UL RTI, Electrical  65.0 °C
@Thickness 0.800 mm
149 °F
@Thickness 0.0315 in
Conditioned; UL 746 B
 65.0 °C
@Thickness 0.800 mm
149 °F
@Thickness 0.0315 in
Dry as Molded; UL 746 B
UL RTI, Mechanical with Impact  65.0 °C
@Thickness 0.800 mm
149 °F
@Thickness 0.0315 in
Conditioned; UL 746 B
 65.0 °C
@Thickness 0.800 mm
149 °F
@Thickness 0.0315 in
Dry as Molded; UL 746 B
UL RTI, Mechanical without Impact  65.0 °C
@Thickness 0.800 mm
149 °F
@Thickness 0.0315 in
Conditioned; UL 746 B
 65.0 °C
@Thickness 0.800 mm
149 °F
@Thickness 0.0315 in
Dry as Molded; UL 746 B
Flammability, UL94  V-2
@Thickness 0.400 mm
V-2
@Thickness 0.0157 in
Conditioned
 V-2
@Thickness 0.400 mm
V-2
@Thickness 0.0157 in
Dry as Molded
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Dry as Molded
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
Dry as Molded
 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
Dry as Molded
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Conditioned
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
Conditioned
 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
Conditioned
Oxygen Index 32 %32 %Conditioned; ISO 4589-1/2
 32 %32 %Dry as Molded; ISO 4589-1/2
Glow Wire Ignition Temperature  750 °C
@Thickness 0.800 mm
1380 °F
@Thickness 0.0315 in
Conditioned; IEC 60695-2-13
 750 °C
@Thickness 1.60 mm
1380 °F
@Thickness 0.0630 in
Dry as Molded; IEC 60695-2-13
 750 °C
@Thickness 0.800 mm
1380 °F
@Thickness 0.0315 in
Dry as Molded; IEC 60695-2-13
 750 °C
@Thickness 1.60 mm
1380 °F
@Thickness 0.0630 in
Conditioned; IEC 60695-2-13
 775 °C
@Thickness 0.400 mm
1430 °F
@Thickness 0.0157 in
Conditioned; IEC 60695-2-13
 775 °C
@Thickness 3.20 mm
1430 °F
@Thickness 0.126 in
Conditioned; IEC 60695-2-13
 775 °C
@Thickness 0.400 mm
1430 °F
@Thickness 0.0157 in
Dry as Molded; IEC 60695-2-13
 775 °C
@Thickness 3.20 mm
1430 °F
@Thickness 0.126 in
Dry as Molded; IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
Conditioned; IEC 60695-2-12
 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
Conditioned; IEC 60695-2-12
 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
Conditioned; IEC 60695-2-12
 960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
Conditioned; IEC 60695-2-12
 960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
Dry as Molded; IEC 60695-2-12
 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
Dry as Molded; IEC 60695-2-12
 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
Dry as Molded; IEC 60695-2-12
 960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
Dry as Molded; IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKRO9929 / 255586

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.