MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Mitsubishi Chemical Advanced Materials Altron™ PPO Polyphenylene oxide, unfilled, extruded (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Water Absorption 0.10 %0.10 %Immersion, 24hr; ASTM D570(2)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9292ASTM D785
Tensile Strength 57.2 MPa8300 psiASTM D638
Tensile Strength at 65°C (150°F) 27.6 MPa4000 psiASTM D638
Elongation at Break 23 %23 %ASTM D638
Tensile Modulus 2.53 GPa367 ksiASTM D638
Flexural Strength 88.9 MPa12900 psiASTM D790
Flexural Modulus 2.74 GPa397 ksiASTM D790
Compressive Strength 91.0 MPa13200 psi10% Def.; ASTM D695
Compressive Modulus 2.18 GPa316 ksiASTM D695
Shear Strength 57.2 MPa8300 psiASTM D732
Izod Impact, Notched 1.55 J/cm2.90 ft-lb/inASTM D256 Type A
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1e+13 ohm>= 1e+13 ohmEOS/ESD S11.11
Dielectric Strength 27.6 kV/mm701 kV/inShort Term; ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 64.1 µm/m-°C
@Temperature -40.0 - 149 °C
35.6 µin/in-°F
@Temperature -40.0 - 300 °F
ASTM E831
Maximum Service Temperature, Air 93.3 °C200 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 127 °C260 °FASTM D648
Glass Transition Temp, Tg 140 °C284 °FASTM D3418
Flammability, UL94 V-1
@Thickness 3.17 mm
V-1
@Thickness 0.125 in
Estimated Rating
 
Compliance PropertiesMetricEnglishComments
3A-Dairy NoNo
Canada AG NoNo
FDA NoNo
USDA NoNo
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) UnacceptableUnacceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents UnacceptableUnacceptable
Conductive / Static Dissipative NoNo
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic LimitedLimited
Hydrocarbons - Aromatic UnacceptableUnacceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters UnacceptableUnacceptable
 
Descriptive Properties
ColorBlack
Machinability61-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger NORYL® Polyphenylene oxide (PPO)
Overview of materials for PPE/PPO + Carbon Fiber
BASF Ultramid® 1503-2 NF2004 33% Glass Filled PA66 (Conditioned)
Mitsubishi Chemical Advanced Materials Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet)
EPICHEM Epiryl PPO V0 Polyphenylene oxide

P1SM10A / 20085

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.