MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ascend Performance Materials Starflam® 315J BK0707 PA66/6 FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Starflam 315J BK0707 (formerly Vydyne® ECO315J BK0707) is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. 315J BK0707 is also lubricated for machine feed and easy mold release.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³DAM; ISO 1183
Water Absorption 0.80 %
@Time 86400 sec
0.80 %
@Time 24.0 hour
DAM; ISO 62
Moisture Absorption at Equilibrium 2.3 %2.3 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.012 cm/cm
@Thickness 2.00 mm
0.012 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.014 cm/cm
@Thickness 2.00 mm
0.014 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 42.0 MPa6090 psi50% RH; ISO 527-2
 75.0 MPa10900 psiDAM; ISO 527-2
Elongation at Break 22 %22 %DAM; ISO 527-2
 140 %140 %50% RH; ISO 527-2
Elongation at Yield 3.5 %3.5 %DAM; ISO 527-2
 23 %23 %50% RH; ISO 527-2
Tensile Modulus 1.20 GPa174 ksi50% RH; ISO 527-2
 3.25 GPa471 ksiDAM; ISO 527-2
Flexural Strength 45.0 MPa6530 psi50% RH; ISO 178
 92.0 MPa13300 psiDAM; ISO 178
Flexural Modulus 1.56 GPa226 ksi50% RH; ISO 178
 3.20 GPa464 ksiDAM; ISO 178
Poissons Ratio 0.400.40ISO 527-2
Izod Impact, Notched (ISO) 6.00 kJ/m²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.540 J/cm²
@Temperature -30.0 °C
2.57 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.540 J/cm²
@Temperature 23.0 °C
2.57 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm
@Thickness 1.00 mm
1.00e+11 ohm-cm
@Thickness 0.0394 in
DAM; IEC 60093
Dielectric Strength 13.0 kV/mm
@Thickness 1.00 mm
330 kV/in
@Thickness 0.0394 in
DAM; IEC 60243
Arc Resistance 120 - 180 sec
@Thickness 3.00 mm
120 - 180 sec
@Thickness 0.118 in
PLC 5; ASTM D 495
Comparative Tracking Index 600 V
@Thickness 3.00 mm
600 V
@Thickness 0.118 in
IEC 60112
Hot Wire Ignition, HWI 7.0 - 15 sec7.0 - 15 secPLC 4; UL 746
 7.0 - 15 sec7.0 - 15 secPLC 4; UL 746
 7.0 - 15 sec7.0 - 15 secPLC 4; UL 746
 15 - 30 sec15 - 30 secPLC 3; UL 746
High Amp Arc Ignition, HAI >= 120 arcs>= 120 arcsPLC 0; UL 746
 >= 120 arcs>= 120 arcsPLC 0; UL 746
 >= 120 arcs>= 120 arcsPLC 0; UL 746
 >= 120 arcs>= 120 arcsPLC 0; UL 746
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min0.394 - 1.00 in/minPLC 1; UL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
61.1 µin/in-°F
@Thickness 0.0787 in,
Temperature 95.0 - 131 °F
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
61.1 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
DAM; ISO 11359-2
Melting Point 244 °C471 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 225 °C437 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical  130 °C
@Thickness 0.400 mm
266 °F
@Thickness 0.0157 in
UL 746
 130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746
 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
UL 746
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  65.0 °C
@Thickness 0.400 mm
149 °F
@Thickness 0.0157 in
UL 746
 65.0 °C
@Thickness 0.750 mm
149 °F
@Thickness 0.0295 in
UL 746
 85.0 °C
@Thickness 1.50 mm
185 °F
@Thickness 0.0591 in
UL 746
 85.0 °C
@Thickness 3.00 mm
185 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  100 °C
@Thickness 0.400 mm
212 °F
@Thickness 0.0157 in
UL 746
 100 °C
@Thickness 0.750 mm
212 °F
@Thickness 0.0295 in
UL 746
 100 °C
@Thickness 1.50 mm
212 °F
@Thickness 0.0591 in
UL 746
 110 °C
@Thickness 3.00 mm
230 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
Oxygen Index 29 %29 %DAM; EN ISO 4589-2
Glow Wire Ignition Temperature  725 °C
@Thickness 3.00 mm
1340 °F
@Thickness 0.118 in
IEC 60695-2-13
 775 °C
@Thickness 1.50 mm
1430 °F
@Thickness 0.0591 in
IEC 60695-2-13
 875 °C
@Thickness 0.400 mm
1610 °F
@Thickness 0.0157 in
IEC 60695-2-13
 875 °C
@Thickness 0.750 mm
1610 °F
@Thickness 0.0295 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
IEC 60695-2-12
 960 °C
@Thickness 0.750 mm
1760 °F
@Thickness 0.0295 in
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 240 - 270 °C464 - 518 °FInjection
Middle Barrel Temperature 240 - 270 °C464 - 518 °FInjection
Front Barrel Temperature 240 - 270 °C464 - 518 °FInjection
Nozzle Temperature 240 - 270 °C464 - 518 °FInjection
Melt Temperature 250 - 270 °C482 - 518 °FInjection
Mold Temperature 65.0 - 95.0 °C149 - 203 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 4.00 hour4.00 hourInjection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Heat Stabilizer
 Lubricant
AppearanceBlack
FeaturesCrack Resistant
 Ductile
 Flame Retardant
 Good Mold Release
 Good Toughness
 Halogen Content, None
 High Elongation
 Low Density
 Lubricated
 Organic Heat Stabilized
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific
Suggested Max Regrind (%)50Injection
UL File NumberE70062

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE9102 / 287553

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.