MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ascend Performance Materials Vydyne® R435H BK0757 PA66-I-GF35
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Reinforced, Impact Grade

Material Notes: Vydyne R435H BK0757, is designed to reinforce downgauged steel and aluminum used in vehicle body-in-white (BIW) structures, helping reduce weight without sacrificing safety or comfort.R435H BK0757 has improved energy absorption over traditional glass-filled PA66, helping reduce noise, vibration and harshness (NVH) and absorbing impact energy from crashes. Using the new grade in the BIW structure reinforces sheet metal, helping manufacturers shave substantial weight and improve efficiency. Trends in lightweight and NVH are becoming even more paramount with the growth of Electric Vehicles. R435H BK0757 has excellent properties to support applications where this will be of prime importance such as battery frames and housings.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³DAM; ISO 1183
Moisture Absorption at Equilibrium 1.38 %1.38 %DAM to 50% RH; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 173 MPa25100 psiDAM; ISO 527-2
Elongation at Break 2.9 %2.9 %DAM; ISO 527-2
Tensile Modulus 11.3 GPa1640 ksiDAM; ISO 527-2
Flexural Strength 260 MPa37700 psiDAM; ISO 178
Flexural Modulus 10.1 GPa1460 ksiDAM; ISO 178
Izod Impact, Notched (ISO)  13.0 kJ/m²
@Temperature -40.0 °C
6.19 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 17.0 kJ/m²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Charpy Impact Unnotched  9.30 J/cm²
@Temperature 23.0 °C
44.3 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
 9.80 J/cm²
@Temperature -40.0 °C
46.6 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  1.40 J/cm²
@Temperature -40.0 °C
6.66 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 248 °C478 °FUnannealed; DAM; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Middle Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Front Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Nozzle Temperature 280 - 310 °C536 - 590 °FInjection
Melt Temperature 285 - 305 °C545 - 581 °FInjection
Mold Temperature 65.0 - 95.0 °C149 - 203 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 4.00 hour4.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
Agency RatingsASTM, D4066 PA016G35
 ASTM, D6779 PA016G35
AppearanceBlack
FeaturesBalanced Stiffness/Toughness
 Chemical Resistant
 Gasoline Resistant
 Good Dimensional Stability
 Good Heat Resistance
 Good Rigidity
 Good Tensile Strength
 Good Toughness
 Impact Modified
 Lubricated
 Oil Resistant
 Solvent Resistant
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE9296 / 287646

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.