MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

LG Chemical LUMILOY GP2100 mPPE, 10% Glass Fiber reinforced, Injection Molding Grade, Flame Retardant
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, 10% Glass Filled

Material Notes: GF 10% Reinforced, High Flow, High Impact Strength, Hydrolytic Stability

Application: Electric and Electronic parts, Part for Water contact, Water pump Housing or Impellers

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
0.0030 - 0.0050 in/in
@Thickness 0.126 in
ISO294-4
Linear Mold Shrinkage, Transverse 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0080 in/in
@Thickness 0.126 in
ISO294-4
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 280 °C
13 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 81.4 MPa
@Thickness 3.20 mm
11800 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break 5.0 %
@Thickness 3.20 mm
5.0 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Strength 157 MPa
@Thickness 3.20 mm
22800 psi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Flexural Modulus 3.96 GPa
@Thickness 3.20 mm
575 ksi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Izod Impact, Notched 0.981 J/cm
@Thickness 3.20 mm
1.84 ft-lb/in
@Thickness 0.126 in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm
@Thickness 3.20 mm
10.0 ft-lb/in
@Thickness 0.126 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
@Thickness 3.20 mm
277 °F
@Thickness 0.126 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 300 °C500 - 572 °F
Middle Barrel Temperature 270 - 310 °C518 - 590 °F
Front Barrel Temperature 270 - 310 °C518 - 590 °F
Nozzle Temperature 270 - 310 °C518 - 590 °F
Melt Temperature 280 - 320 °C536 - 608 °F
Mold Temperature 70.0 - 110 °C158 - 230 °F
Drying Temperature 90.0 - 100 °C
@Time 14400 - 21600 sec
194 - 212 °F
@Time 4.00 - 6.00 hour
Moisture Content <= 0.020 %<= 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLHCHEM9770 / 239286

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.