MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Dow Appeel® 22D843 Ethylene Acrylate
Categories: Polymer; Thermoplastic; Ethylene Acrylic Acid

Material Notes: DuPont™ Appeel® 22D843 is a polypropylene modified ethylene acrylate resin designed to function as a masterbatch to achieve peelability in polypropylene based sealant layers. It provides peelable seals over a broad temperature range. The peel layers will sustain sterilization conditions of 121°C for 20 minutes through 134°C for 6 minutes depending on the base of the PP seal materials. When blending for this type of application, 22D843 should be evaluated as a modifier for HoPP or CoPP by addition rates between 20% to 40% by weight. Blends with CoPP will usually provide better results. Appeel® 22D843 is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene resins.

Appeel® 22D843 Lidding Sealant Resin complies with Food and Drug Administration Regulation 21 CFR 177.1340 - - Ethylene-methyl acrylate copolymer resins, subject to the limitations and requirements therein. Appeel® 22D843 Lidding Sealant Resin may be used in non-cooking applications under conditions corresponding to Conditions of Use C (Hot filled or Pasteurized above 150F, includes microwave reheating) through G (frozen storage, no thermal treatment in the container) (21 CFR 176.170, Table 2, subject to the finished food-contact article meeting the extractive limitations under the intended conditions of use, as shown in paragraph 21 CFR 177.1340 paragraph (b). Appeel® 22D843 Lidding Sealant Resin may also be used for packaging all food types in a cooking application at a maximum thickness of 3.5 mils in pouches under retort conditions only, corresponding to Condition of Use A (21 CFR 176.170, Table 2), subject to the finished food-contact article meeting the extractive limitations under the intended conditions of use, as shown in paragraph 21 CFR 177.1340 paragraph (b). Such use may properly be said to comply with Federal Food, Drug and Cosmetic Act and all applicable food additive regulations.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.937 g/cc0.0339 lb/in³ASTM D792, ISO 1183
Melt Flow  2.6 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.6 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
 6.4 g/10 min
@Load 2.16 kg,
Temperature 230 °C
6.4 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238, ISO 1133
 
Thermal PropertiesMetricEnglishComments
Melting Point 136 °C277 °FASTM D3418, ISO 3146
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 300 °C<= 572 °F
Feed Temperature 140 °C284 °FBlown Film Coextrusion
Zone 2 150 °C302 °FBlown Film Coextrusion
Zone 3 160 °C320 °FBlown Film Coextrusion
Zone 4 180 °C356 °FBlown Film Coextrusion
Zone 5 180 °C356 °FBlown Film Coextrusion
Adapter Temperature 180 °C356 °FBlown Film Coextrusion
Die Temperature 170 °C338 °FBlown Film Coextrusion
Melt Temperature 160 - 185 °C320 - 365 °FBlown Film Coextrusion
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Ethylene Acrylic Acid
Dow Primacor® 1410 Ethylene Acrylic Acid (EAA)
Dow Appeel® 20D784 Ethylene Acrylate
Dow Appeel® 20D828 Ethylene Acrylate
Dow Primacor® 1420 Ethylene Acrylic Acid (EAA)

PDTA4907 / 170347

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.