MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Polymer Resources PPX-G5 Modified-PPO, 5% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, 10% Glass Filled

Material Notes: Modified-Polyphenylene Oxide, 5% Glass Reinforced

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Key Words: Polyphenylene Ether + PS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inASTM D955
Melt Flow 2.0 - 10 g/10 min
@Load 11.6 kg,
Temperature 250 °C
2.0 - 10 g/10 min
@Load 25.6 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 62.1 MPa9000 psiASTM D638
Tensile Strength, Yield 63.8 MPa9250 psiASTM D638
Elongation at Break 6.0 %6.0 %ASTM D638
Flexural Strength 96.5 MPa14000 psiASTM D790
Flexural Modulus 2.93 GPa425 ksiASTM D790
Izod Impact, Notched  1.07 J/cm
@Temperature -30.0 °C
2.00 ft-lb/in
@Temperature -22.0 °F
ASTM D256
 1.60 J/cm
@Temperature 22.8 °C
3.00 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 127 °C260 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 121 °C250 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 304 °C500 - 580 °F
Middle Barrel Temperature 271 - 310 °C520 - 590 °F
Front Barrel Temperature 282 - 316 °C540 - 600 °F
Melt Temperature 288 - 316 °C550 - 600 °F
Mold Temperature 71.1 - 104 °C160 - 220 °F
Drying Temperature 104 - 110 °C220 - 230 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Vent Depth 0.00381 cm0.00150 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 1799 X 138211 C Modified Polyphenylene Oxide (PPO); Glass Fiber - Flame Retardant
RTP Company RTP 1701 Modified Polyphenylene Oxide (PPO), Glass Fiber
Polymer Resources PPX-MF-FR1 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced
Nylene® Norpex® AX10GF 10% Glass Reinforced Polyphenylene Ether

PPOLYQ218a / 160740

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.