MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Evonik VESTAMID® L-GF30 black 9.7506 Nylon 12, 30% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 30% Glass Fiber Filled

Material Notes: VESTAMID® L-GF30 black 9.7506 is a glass fiber–reinforced heat stabilized Polyamide 12 for injection molding. The material contains about 30% glass fibers, an ageing protective agent and a processing aid for a fast and even form filling. Due to the reinforcement moldings from this compound exhibit a higher strength and good heat resistance. Further advantages of VESTAMID® L-GF30 black 9.7506 are the characteristic properties of PA12, e.g., low water absorption, good dimensional stability and nearly constant mechanical properties at changing ambient humidity. VESTAMID® L-GF30 black 9.7506 is supplied as cylindrical granules, ready for processing, in moisture-proof bags. Pigmentation may affect values.

Property data for dry samples unless otherwise noted.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ISO 1183
Water Absorption 1.1 %1.1 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inISO 294-4, 2577
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 275 °C
13 g/10 min
@Load 4.76 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 111 MPa16100 psiISO 527
Tensile Strength, Yield 114 MPa16500 psiISO 527
Elongation at Break 5.0 %5.0 %ISO 527
Elongation at Yield 4.0 %4.0 %ISO 527
Tensile Modulus 6.80 GPa986 ksiISO 527
Charpy Impact Unnotched  8.50 J/cm²
@Temperature 23.0 °C
40.4 ft-lb/in²
@Temperature 73.4 °F
Complete Break; ISO 179/1eU
 10.0 J/cm²
@Temperature -40.0 °C
47.6 ft-lb/in²
@Temperature -40.0 °F
Complete Break, Conditioned; ISO 179/1eU
Charpy Impact, Notched  2.10 J/cm²
@Temperature -30.0 °C
9.99 ft-lb/in²
@Temperature -22.0 °F
Complete Break; ISO 179/1eA
 2.30 J/cm²
@Temperature 23.0 °C
10.9 ft-lb/in²
@Temperature 73.4 °F
Complete Break; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmIEC 62631-3-1
Dielectric Constant 3.4
@Frequency 1e+6 Hz
3.4
@Frequency 1e+6 Hz
Sim. to IEC 60243-1
Dissipation Factor 0.023
@Frequency 1e+6 Hz
0.023
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 600 V600 Vtest solution A, 100 drops value; IEC 60112
 600 V600 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
33.3 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2.
Melting Point 178 °C352 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 175 °C347 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 165 °C329 °FISO 75-1/-2
Vicat Softening Point 175 °C347 °FMethod A: 10 N, 50 K/h; ISO 306
 175 °C347 °FMethod B: 10 N, 50 K/h; ISO 306
Flammability Test  1.0
@Thickness 1.60 mm
1.0
@Thickness 0.0630 in
IEC 60695-11-10
 1.0
@Thickness 3.20 mm
1.0
@Thickness 0.126 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 °C482 °FTest condition for mold shrinkage
Mold Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK842 / 243051

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.