MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Corning Ba PC 701 Photochromic Barium Glass, Code 8088
Categories: Ceramic; Glass; Optical

Material Notes: Application : Near vision segments for fused multifocal lenses

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.08 g/cc0.147 lb/in³
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.50 µm/m-°C3.61 µin/in-°F
Softening Point 632 °C1170 °F
Annealing Point 500 °C932 °F
Strain Point 632 °C1170 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.7011.701
Transmission, Visible 86.7 %86.7 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Polylac® PA-757 ABS
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Mitsubishi Chemical Advanced Materials TIVAR® HPV Food Grade UHMW-PE (ASTM Product Data Sheet)
Corning Borosilicate Specialty Glass Pressed Parts
Corning B 17 Tinted Optical Glass

CCORN933 / 233344

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.