MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Celanese Minlon® 10B40 NC010 PA66-MD40
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Mineral Filled

Material Notes: 40% Mineral Reinforced Polyamide 66

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³DAM; ISO 1183
Water Absorption 5.0 %
@Thickness 2.00 mm
5.0 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 1.60 %
@Thickness 2.00 mm
1.60 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 58.0 MPa8410 psi50% RH; ISO 527-1/-2
 92.0 MPa13300 psiDAM; ISO 527-1/-2
Elongation at Break 2.5 %2.5 %DAM; ISO 527-1/-2
 8.0 %8.0 %50% RH; ISO 527-1/-2
Tensile Modulus 5.40 GPa783 ksi50% RH; ISO 527-1/-2
 9.60 GPa1390 ksiDAM; ISO 527-1/-2
Flexural Modulus 4.80 GPa696 ksi50% RH; ISO 178
 9.00 GPa1310 ksiDAM; ISO 178
Poissons Ratio 0.340.34DAM
 0.350.3550% RH
Izod Impact, Notched (ISO)  2.00 kJ/m²
@Temperature -30.0 °C
0.952 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 2.00 kJ/m²
@Temperature -40.0 °C
0.952 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 180/1A
 2.50 kJ/m²
@Temperature -40.0 °C
1.19 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 2.50 kJ/m²
@Temperature -30.0 °C
1.19 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 3.50 kJ/m²
@Temperature 23.0 °C
1.67 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 4.00 kJ/m²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Izod Impact, Unnotched (ISO)  18.0 kJ/m²
@Temperature -30.0 °C
8.57 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1U
 18.0 kJ/m²
@Temperature -30.0 °C
8.57 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1U
 25.0 kJ/m²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1U
 40.0 kJ/m²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1U
Charpy Impact Unnotched  1.70 J/cm²
@Temperature -30.0 °C
8.09 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 1.80 J/cm²
@Temperature -30.0 °C
8.57 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eU
Charpy Impact, Notched  0.200 J/cm²
@Temperature -40.0 °C
0.952 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eA
 0.200 J/cm²
@Temperature -40.0 °C
0.952 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 0.200 J/cm²
@Temperature -30.0 °C
0.952 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 0.200 J/cm²
@Temperature -30.0 °C
0.952 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
Tensile Creep Modulus, 1 hour 2500 MPa363000 psi1h; 50% RH; ISO 899-1
Tensile Creep Modulus, 1000 hours 1600 MPa232000 psi1000h; 50% RH; ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmDAM; IEC 62631-3-1
Surface Resistance 1.00e+15 ohm1.00e+15 ohm50% RH; IEC 62631-3-2
Dielectric Strength 30.0 kV/mm762 kV/inDAM; IEC 60243-1
Dissipation Factor  0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
DAM; IEC 62631-2-1
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 36.0 µm/m-°C20.0 µin/in-°FDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 66.0 µm/m-°C36.7 µin/in-°FDAM; ISO 11359-1/-2
Melting Point 263 °C505 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 245 °C473 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FDAM; ISO 75-1/-2
Flammability, UL94  HB
@Thickness 0.710 mm
HB
@Thickness 0.0280 in
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
DAM; IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Oxygen Index 23 %23 %DAM; ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 295 °C563 °FOptimum, Injection
 285 - 305 °C545 - 581 °FRange, Injection
Mold Temperature 70.0 - 120 °C158 - 248 °FInjection
 100 °C212 °FOptimum, Injection
Ejection Temperature 210 °C410 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %<= 0.20 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiInjection
 100 MPa14500 psiInjection
 
Descriptive Properties
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA66,MD40,M1GN,S14-100
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PA66-MD40<ISO 11469
PolymerPA66-MD40
Processing Hold Pressure Time (s/mm)3Injection
Regional AvailabilityAsia Pacific
 North America
 South and Central America
Resin IdentificationPA66-MD40ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® 101L BKB009 PA66
Overview of materials for Nylon 66, 20% Glass Fiber Filled
Celanese Zytel® 101F BKB009 PA66
BASF Ultramid® N-265 NF3001 40% Mineral Filled PA66 (Dry)
Celanese Zytel® 101 NC010 PA66

PDSX5238 / 197878

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.