MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Celanese VECTRA S475 LCP, 32% Mineral / Glass Reinforced
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled

Material Notes: Super High Flow, High heat Resistance and Low Warp for Thin Parts.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.65 g/cc0.0596 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.00 cm/cm0.00 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0037 cm/cm0.0037 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 135 MPa19600 psi5mm/min; ISO 527-2/1A
Elongation at Break 1.8 %1.8 %5mm/min; ISO 527-2/1A
Tensile Modulus 12.3 GPa1780 ksi50mm/min; ISO 527-2/1A
Flexural Strength 180 MPa26100 psiISO 178
Flexural Modulus 12.0 GPa1740 ksiISO 178
Flexural Strain at Break 2.4 %2.4 %ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 1.45 J/cm²6.90 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
IEC 60250
 3.95
@Frequency 2.05e+9 Hz
3.95
@Frequency 2.05e+9 Hz
Dissipation Factor  0.0080
@Frequency 1e+6 Hz
0.0080
@Frequency 1e+6 Hz
IEC 60250
 0.010
@Frequency 2.05e+9 Hz
0.010
@Frequency 2.05e+9 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C5.56 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 25.0 µm/m-°C13.9 µin/in-°FISO 11359-2
Melting Point 350 °C662 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 305 °C581 °FISO 75-1, -2
Deflection Temperature at 8.0 MPa 213 °C415 °FISO 75-1, -2
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 120 °C176 - 248 °Fcavity
 355 - 370 °C671 - 698 °Fhot runner
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Zone 1 330 - 350 °C626 - 662 °F
Zone 2 340 - 360 °C644 - 680 °F
Zone 3 345 - 365 °C653 - 689 °F
Zone 4 355 - 370 °C671 - 698 °F
Die Temperature 355 - 370 °C671 - 698 °F
Melt Temperature 360 - 375 °C680 - 707 °F
Drying Temperature >= 150 °C>= 302 °F
Dry Time 6.00 hour6.00 hour
Moisture Content <= 0.010 %<= 0.010 %
Injection Pressure 50.0 - 150 MPa7250 - 21800 psi
Hold Pressure 50.0 - 150 MPa7250 - 21800 psi
Back Pressure <= 3.00 MPa<= 435 psi
Screw Speed  80 rpm
@Diameter 40.0 mm
80 rpm
@Diameter 1.57 in
 120 rpm
@Diameter 25.0 mm
120 rpm
@Diameter 0.984 in
 200 rpm
@Diameter 16.0 mm
200 rpm
@Diameter 0.630 in
 
Descriptive Properties
Injection speedmedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
Celanese VECTRA S471 LCP, 45% Mineral / Glass Reinforced
Celanese VECTRA E130i LCP, 30% Glass Reinforced
Celanese VECTRA E473i LCP, 32% Mineral / Glass Reinforced
Celanese VECTRA S135 LCP, 35% Glass Reinforced

PHCQ526 / 178981

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.