MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Envalior Pocan® A 3122 901510 PBT+ASA, 20% Glass Fiber
Categories: Polymer; Thermoplastic; ASA Polymer; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + ASA Blend, Glass Fiber Reinforced

Material Notes: PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finish

Former Lanxess product line is now with Envalior.

Key Words: ISO 7792-1-PBT+ASA, GHMR, 07-060, GF20
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.700 g/cc0.0253 lb/in³ISO 60
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/in60x60x2; 270°C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in60x60x2; 270°C / MT 80°C; 600 bar; ISO 294-4
Melt Flow 30.8 g/10 min
@Load 2.16 kg,
Temperature 270 °C
30.8 g/10 min
@Load 4.76 lb,
Temperature 518 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psi5 mm/min; ISO 527-1,-2
Elongation at Break 2.9 %2.9 %5 mm/min; ISO 527-1,-2
 3.2 %3.2 %50 mm/min; ISO 527-1,-2
Tensile Modulus 6.50 GPa943 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 165 MPa23900 psi2 mm/min; ISO 178-A
Flexural Modulus 6.20 GPa899 ksi2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  <= 10.0 kJ/m²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)  40.0 kJ/m²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
 45.0 kJ/m²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched  4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched  <= 1.00 J/cm²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eA
 <= 1.00 J/cm²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °F10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 185 °C365 °FISO 75-1,-2
Vicat Softening Point 170 °C338 °F50 N; 50 °C/h; ISO 306
Shrinkage  0.10 %
@Temperature 120 °C,
Time 14400 sec
0.10 %
@Temperature 248 °F,
Time 4.00 hour
post-shrinkage, transverse, 60x60x2; ISO 294-4
 0.20 %
@Temperature 120 °C,
Time 14400 sec
0.20 %
@Temperature 248 °F,
Time 4.00 hour
post-shrinkage, 60x60x2; ISO 294-4
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 °C518 °FInjection molding; ISO 294
Mold Temperature 90.0 °C194 °FInjection molding; ISO 294
Dry Time 4.00 - 8.00 hour
@Temperature 120 °C
4.00 - 8.00 hour
@Temperature 248 °F
Moisture Content 0.00 - 0.020 %0.00 - 0.020 %Karl Fischer test

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Pocan® TP 740-202 901510 PBT+ASA, 20% Glass Fiber
Envalior Pocan® A 3121 000000 PBT+ASA, 20% Glass Fiber Reinforced
Envalior Pocan® BF 4222 000000 PBT, 20% Glass Fiber Reinforced
Envalior Pocan® DP CF 2200 000000 PBT+PC
MBA Polymers PS 3122 Post-consumer recycled impact modified polystyrene

PLANX0520 / 150479

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.